Date recorded: May 18 2010

Duration: 13 minutes 48 seconds

Triple detection is used with size-exclusion chromatography to characterize the absolute molecular weight and molecular size of synthetic and biological macromolecules independent of each other, and without relying on retention time
Table of contents
1. Polymer Characterization by Triple or Tetra Detection SEC/GPC
00:23
2. Size-Exclusion Chromatography (SEC)
01:27
3. Triple/Tetra Detection SEC by Malvern
01:28
4. Concentration Detectors
01:59
5. Advanced UV Plots Available with PDA
01:01
6. Solution Viscometry - Four-capillary Viscometer
00:59
7. Structure Analysis – Mark-Houwink Plots
00:55
8. Static Light Scattering for SEC
01:15
9. Triple/Tetra Detection Principles
01:28
10. Advanced Polymer Analysis Using Triple Detection
02:00
11. Triple/Tetra Detection - Summary
00:53