See the current Axios Fast range . Learn more

Learn more

Axios FAST

The Malvern Panalytical Axios FAST simultaneous WDXRF spectrometer is the ideal tool for time-critical applications and high sample throughput analysis environments. Main application areas include steel and metals alloy production as well as geological or commercial laboratories where hundreds of samples need to be analyzed every day.

Looking for more information?

To request a quote, more information or download a brochure select an option below.

Manuals

Title Version Date Product Download
{{ row.title }} {{ row.softwareVersion }} {{ row.date }}
{{ product }}
Download

Sorry, no manuals are available for this product

Software

Title Version Date Product Download
{{ row.title }} {{ row.softwareVersion }} {{ row.date }}
{{p}}
Download

Sorry, no software downloads are available for this product

Accessories

Standards (reference materials)

Cu-base-FP

Accurate elemental analysis of Cu metals

‘Copper-base’ (Cu-base) is a term used to describe a range of alloys where Cu is the principal component. In order to make the materials suitable for different applications (e.g. the manufacture of coinage, bells, a wide range of mechanical equipment and electrical wiring), Cu is normally alloyed with elements such as Sn, Zn, Ni, Al, and Pb. During the production process fast chemical analysis is needed to minimize errors in production and to maximize production yield. The Cu-base-FP package (including applicable calibration standards) covers the analysis of this wide range of Cu alloys by using the Fundamental Parameter (FP) model.

CRMs

Claisse is always there to meet your needs!

Claisse provides its customers with quality Certified Reference Materials (CRM) and Reference Materials (RM) from around the world at competitive prices. Whatever your needs, Claisse strives to provide you with the all around services needed to obtain the perfect solution for your XRF, AA and ICP spectroscopy analysis.

Fused Borate Disks

Calibration made easy!

Customized Fused Borate Disks for the calibration and monitoring of XRF applications.

Claisse has a new turn-key solution for your XRF applications. Our fused borate disks are made with Certified Reference Materials (CRM) or customized mixtures of synthetic oxides. They are custom-made to fulfill your personal analytical needs.

NiFeCO

The NiFeCo module and setup samples are ideal for calibrating your AxiosFAST instrument for the analysis of high temperature steels and super alloys.    

Fluxes and Chemicals

Borate fluxes and chemicals

Your first choice to fuse samples for XRF, ICP and AA analysis

As the one-stop shop in fusion and the world leader in the production of borate fluxes, Claisse develops high-quality chemicals that are easy to use and that ensure no contamination.

Offered in two grades of purity (pure 99.98+% and ultra pure 99.995+%) and available with or without non-wetting agents, our lithium borate fluxes are homogeneous and available in bead format.

Use Claisse lithium borate fluxes to:

  • Avoid crystallization
  • Reduce the incidence of glass sticking to the platinumware
  • Avoid cracking

Make your life easier, try our pre-weighed or customized borate fluxes.

Fusion monitor

Quick and error-free proactive monitoring for your fusion instruments

XRF laboratories must assure the quality of their analytical results and ensure accurate and precise data by using quality control sample regularly.

Obtaining the wrong analytical results can affect manufacturing and commercial decisions which can be very costly. Moreover, the Fusion-XRF process remains offline until the source of the variability is thoroughly identified and eliminated. When the analytical results are found to be outside the predefined criteria, planned actions must be taken. Since the analytical results can be affected by a large number of factors, troubleshooting steps may oftentimes become expensive and time consuming.

Platinum and Labware

Platinum molds and crucibles

Labware is of critical importance in sample preparation by fusion. Malvern Panalytical offers molds and crucibles made of 95% platinum are 5% gold. They are available in a wide range of sizes and thicknesses to help you obtain the best analytical results.

We also offer nickel and zirconium crucibles for peroxide fusion.

Malvern Panalytical fusion instruments were developed to be used with specifically designed platinumware. All our platinum accessories have been tested and engineered to provide:

  • The best mixing performance.
  • Longer lifetime.
  • Higher success rates in preparation of glass disks.
  • Perfect compatibility with our fusion instruments.

Events and training

All events

Class & Workshop | English |

XRF in the Workplace

Products:
Epsilon 4, Zetium, Axios FAST, Axios range
Technology:
Wavelength Dispersive X-ray Fluorescence (WDXRF), X-ray Fluorescence (XRF)
Industry:
Academia, Mining, Minerals, Metals
XRF in the Workplace

Service and Support

Services

Solutions to maximize the return on your investment

To assure that your instrument remains in top condition and performs on the highest level, Malvern Panalytical offers a wide range of services. Our expertise and support services assure the optimal functioning of your instrument.

Support

Service for a lifetime

  • Phone and remote support
  • Preventive maintenance and checkups
  • Flexible Customer Care Agreements
  • Performance certificates
  • Hardware and software upgrades
  • Local and global support

Expertise

Adding value to your processes 

  • Sample preparation development/optimization
  • Analytical methodologies 
  • Turnkey solutions for XRD 
  • Operations via IQ/OQ/PQ, quality assurance (GLP, ISO17025) or round robins/interlaboratory studies
  • Consultancy services

Training and education

  • Training on-site or at our competence centers
  • Broad range of basic and advanced courses on products, applications and software
Contact support