The Morphologi® automated image analysis system is ideally suited to the efficient characterization of particle size and shape for metal powders used in additive manufacturing and metal injection molding. The quality of the part produced is determined during the sintering stage of the manufacturing process. Even sintering relies on consistent particle packing, which is determined by the size distribution and particle shape. In this application note, the Morphologi was used to determine the shape characteristics of metal powders produced by different methods, but of the same particle size. 