Using the Aeris Research edition, we were able to solve the crystal structure of AgCaVO4 from powder X-ray data in combination with the HighScore software suite. This demonstrates the high data quality which can be achieved with this PANalytical benchtop powder diffractometer.
We investigated the crystal structures of some of these silver vanadates using the Aeris Research edition.