This application overview demonstrates the use of X-ray diffraction in six mining case studies: phase identification of lithium and manganese ores; quantification of heavy mineral sands; quantification of phases in iron ore; quantification of quartz in talc, and quantification and cluster analysis of bauxites.

Valuable information is obtained using state-of-the-art PANalytical technology, including high-speed detectors and advanced software, which illustrates the potential of XRD as a high throughput process control solution. 