Automatic analysis of large amounts of X-ray diffraction data with HighScore Plus

In this application note nano-titania powders from the PANalytical SAXS verification samples kit were measured at various temperatures and analyzed.

When many data sets are obtained during a non-ambient experiment, quick and effective tools are needed for handling and analyzing this data. Tools such as isolines plot, cluster analysis, and fully automated refinements are available and easy to use in HighScore Plus. 