UOP, a Honeywell company, produces test methods used by the petroleum industry to evaluate the performance of catalysts. UOP 979 is a test method to measure the total chloride content in fresh, regenerated and spent aluminasupported catalysts by wavelength dispersive XRF.

This study was performed using the wavelength dispersive optics of the Zetium XRF spectrometer. 