Whilst dynamic light scattering (DLS) is a ubiquitous tool for the characterization of nanomaterials, there may be cases where we want to also know about larger material that might also be present within the sample. Here we will introduce a new analysis model to help characterize particles at sizes not typically measurable via DLS with some examples of the benefits and limitations of this new feature.